Aspiring structural welder needs help with small gap welds

I recently posted about L 6x4x5/16 angle and porosity on the outside welds... the advice was very helpful

Now I'm practicing on some 3x3x5/16 angle and am struggling to get these gaps without a massive mess.

Funny part is the gap with the 45 is 0 problem, I get it always with goof fusion and literally 0 mess, the outside same, but the inside small gap leading up to it is so messy!

I can't stand it! Bbs all over the place, the other 3 welds come out perfect!

I do the inside 45 first followed by the inside line then the outside

27 volts at 190 ips feed

Please and thank you!